Polyteks’ Poly-Optic 14 Part X Accelerator speeds the cure of Poly-Optic products (recommended for castings less than 1/2″ thick). Experiment to determine how much Part X is needed for your application. Do not exceed 1% of the total mixed weight as final physical properties may be affected. Example: 0.5 grams of Part X in a 100 gram mix of Poly-Optic 1410 Clear Casting Resin cuts the pour and cure times in half.
Notes: When Poly-Optic 14 Part X Accelerator is added, exotherm (the heat of the reaction) and thus shrinkage on cooling is also increased. Add Part X to Part B prior to mixing with Part A. For additional information, read the Poly-Optic 14-Series Technical Bulletin.